Mechanical Properties Metric English Comments
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Asia Pacific)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4401R PPC+PC
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region.
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4404 PPC+PC
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific)
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East)
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Impact Test 120 J

@Temperature 23.0 °C
88.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® 4301 PPC+PC
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region.
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer
11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized
Impact Test 120 J
88.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only
Copyright © lookpolymers.com All Rights Reserved