Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 11.3 - 22.6 J | 8.33 - 16.7 ft-lb | Torque Break |
Ritelok TL42 Nutlock Anaerobic. Medium strength threadlocker for screws, nuts and bolts. Prevent corrosion, Vibration resistant, Dismantle using normal tools |
|||
Impact Test | 11.3 - 22.6 J | 8.33 - 16.7 ft-lb | Break |
ND Industries NutGrade® 121 Removable Threadlocker A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th.. |
|||
Impact Test | 11.3 - 14.7 J | 8.33 - 10.8 ft-lb | Break |
ND Industries NutGrade® 122 Removable Threadlocker A medium strength, oil tolerant threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or b.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 260 8 G Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 260 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 262 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 262 is a widely used, well-known general purpose epoxy powder resin. A one-part, red pigmented, rapid heat-curing product, it is designed to provide a continuous, toug.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 263 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 263 is a widely used, well-known general purpose epoxy powder resin. A one part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 5555 22G Electrical Insulating Epoxy Resin 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | Reverse/direct on steel |
Blue River Coatings Steel Seal Primer BLUE RIVER COATINGS STEEL SEAL PRIMER is a high quality, single component primer, not requiring any catalyzing agent. STEEL SEAL PRIMER is designed for dip coaters who need a quick, fast drying pain.. |
|||
Impact Test | 11.3 J | 8.33 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 260 CG Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Impact Test | 11.3 - 22.6 J | 8.33 - 16.7 ft-lb | Torque Break |
Ritelok TL41 Oil Tolerant Threadlocker Anaerobic. Medium strength threadlocker. Designed to lock oily fasteners. Prevent corrosion, Vibration resistant, Dismantle using normal tools |