Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 1.70 J | 1.25 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Impact Test | 1.70 J | 1.25 ft-lb | Spencer Impact ASTM D3420 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |