Mechanical Properties Metric English Comments
300% Modulus 0.00483 - 0.00965 GPa
0.700 - 1.40 ksi
Secant; Conditioned 7 days at RT/50% RH; ASTM D638
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..