Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0200 GPa | 2.90 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go.. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 305ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ASTM D412 |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1190 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 305ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ASTM D412 |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ISO 37 |
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ISO 37 |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1295 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0200 GPa | 2.90 ksi | ISO 37 |
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |