Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0161 GPa | 2.34 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.0161 GPa | 2.34 ksi | DIN 53504 |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
300% Modulus | 0.0161 GPa | 2.34 ksi | ASTM D412 |
Styron Buna® SB 1500 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Composition: Buna® SB 1500 – Schkopau is manufactured by cold polymerization using a rosin acid soap. A discoloring stabilizer is added during the production process.Application: Buna® SB.. |
|||
300% Modulus | 0.0161 GPa | 2.34 ksi | ASTM D412 |
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
300% Modulus | 0.0161 GPa | 2.34 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |