Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0147 GPa | 2.13 ksi | 150°C, 40 min., Pressure Vulcanization. 38% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 0230L Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | 150°C, 40 min., Pressure Vulcanization. 40% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 35M Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | 150°C, 40 min., Pressure Vulcanization. 45% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 40M Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | |
Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | |
Taiwan PU Corporation TPUI-L90 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | |
Taiwan Sheen Soon Sheenthane® A8670A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | |
Taiwan Sheen Soon Sheenthane® A8700F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | |
Taiwan Sheen Soon Sheenthane® A8900F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.0147 GPa | 2.13 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |