Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 1.48 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0102 GPa
1.48 ksi
DIN 53504
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether
Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
300% Modulus 0.0102 GPa
1.48 ksi
ASTM D412
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.0102 GPa
1.48 ksi
ASTM D412
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.0102 GPa
1.48 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR8020 Standard Adipate Ester Polyurethane
The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGr..
Copyright © lookpolymers.com All Rights Reserved