Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00880 GPa | 1.28 ksi | |
Taiwan PU Corporation TPU-E85 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00883 GPa | 1.28 ksi | |
Taiwan Sheen Soon Sheenthane® A8600F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00883 GPa | 1.28 ksi | |
Taiwan Sheen Soon Sheenthane® A8800F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00880 GPa | 1.28 ksi | DIN 53504 |
Lubrizol ESTANE® 58564 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |