Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00779 GPa | 1.13 ksi | ASTM D412 |
Huntsman IROGRAN® PS 370-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
300% Modulus | 0.00780 GPa | 1.13 ksi | |
Taiwan PU Corporation TPU-BH90 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00780 GPa | 1.13 ksi | |
Taiwan PU Corporation TPU-E80 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00780 GPa | 1.13 ksi | |
Taiwan PU Corporation TPU-EH80 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00780 GPa | 1.13 ksi | |
Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00780 GPa | 1.13 ksi | ISO 37 |
Lubrizol ESTANE® 58280 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |