Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00621 GPa | 0.901 ksi | ASTM D412 |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |