Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00331 GPa | 0.480 ksi | |
Taiwan PU Corporation UR50 Polyester Urethane Rubber UR50 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412 |
Teknor Apex TELCAR® 1050-75 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M QI-18/57-325 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M QI-5/16-220 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M SJ-2A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412 |
3M 5300 Motor Lead Splicing Kits 3M Motor Lead Splicing Kits 5300 Series are a series of kits designed for splicing motor lead cables to incoming feeder cables. The kits accommodate the follow splice confiations:Pigtails (stub) con.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8420-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8424-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8425-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8426-11 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8427-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8427-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8428-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8428-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8428-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8429-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8429-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8430-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8453 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8454 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8459 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8462 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M QSLV-M-2-500 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M QSLV-M-8-2/0 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8426-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M 8461 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M EC-2 Cold Shrink End Caps 3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the c.. |
|||
300% Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412-75 |
3M EC-4 Cold Shrink End Caps 3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the c.. |