Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00289 GPa | 0.419 ksi | Injection molded plaques, Die C, Machine Direction; ASTM D412 |
Kraton® G2705 GU (SEBS) Compound Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct.. |
|||
300% Modulus | 0.00289 GPa | 0.419 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00289 GPa | 0.419 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |