Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 499 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
Kraton® D1102 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1102 K (SBS) Liner Block Copolymer Description: Kraton D1102 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 28%. It is supplied from North America in the physical form identified.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
Kraton® D1101 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2770 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2850M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2860E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00276 GPa | 0.400 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |