Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00171 GPa @Time 7200 sec |
0.248 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7050-1000 TPE Product Description: StarMediflex P 7050-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
300% Modulus | 0.00171 GPa | 0.248 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 30A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00171 GPa | 0.248 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 30A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |