Mechanical Properties Metric English Comments
300% Modulus 0.000900 GPa
0.131 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1161 B (SIS) Linear Block Copolymer
Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra..
300% Modulus 0.000900 GPa
0.131 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1161 E (SIS) Linear Triblock Copolymer
Description: Kraton D1161 E is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from Europe in the physical form identified: D1161 E..
300% Modulus 0.000900 GPa
0.131 ksi
ISO 37
Kraton® D1161 J (SIS) Linear Triblock Copolymer
Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t..