Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0352 GPa | 5.10 ksi | ASTM D412 |
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0352 GPa | 5.10 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S368D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0352 GPa | 5.11 ksi | ASTM D412 |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection.. |