Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0196 GPa | 2.84 ksi | |
Taiwan Sheen Soon Sheenthane® A9612K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0196 GPa | 2.84 ksi | |
Taiwan Sheen Soon Sheenthane® A9830 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |