Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0190 GPa | 2.75 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0190 GPa | 2.75 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0190 GPa | 2.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0190 GPa | 2.76 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec.. |
|||
300% Modulus | 0.0190 GPa | 2.76 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7180 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0190 GPa | 2.75 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0190 GPa | 2.76 ksi | ASTM D412 |
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
300% Modulus | 0.0190 GPa | 2.75 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0190 GPa | 2.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0190 GPa | 2.76 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0190 GPa | 2.76 ksi | |
Dow Pellethane® 2354-45D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-45D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane.. |