Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0170 GPa | 2.47 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |
|||
300% Modulus | 0.0170 GPa | 2.47 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
300% Modulus | 0.0170 GPa | 2.47 ksi | ASTM D412 |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
300% Modulus | 0.0170 GPa | 2.47 ksi | Compounded, 35 mins.; ASTM D3185 |
Dynasol Solprene® 303 Random-Block Copolymer Solprene 303 is a linear random-block styrene-butadiene copolymer with 46% styrene content, 11% present as a polystyrene block. S-303 is used in vulcanized microcellular shoe soles, it provides hard.. |