Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0137 GPa | 1.98 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | 150°C, 40 min., Pressure Vulcanization. 35% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 35L Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | |
Taiwan PU Corporation TPUI-H90 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | |
Taiwan PU Corporation TPUI-T85 Transparent Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | |
Taiwan Sheen Soon Sheenthane® A8210F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | |
Taiwan Sheen Soon Sheenthane® A9050 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | |
Taiwan Sheen Soon Sheenthane® A9312R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0137 GPa | 1.98 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.0137 GPa | 1.99 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |