Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0120 GPa | 1.74 ksi | DIN 53504 |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | Measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1118 B (SBS) Linear Triblock Copolymer Description: Kraton D1118 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from South America in the physical form(s) identifi.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ISO 37 |
Kraton® D1118 E (SBS) Diblock Copolymer Description: Kraton D1118 E is a clear, diblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from Europe in the physical form identified: D1118 ET - sup.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ISO 37 |
Huntsman AVALON® 90 AE Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ISO 37 |
Huntsman AVALON® 90 AHT DP Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
300% Modulus | 0.0120 - 0.0180 GPa | 1.74 - 2.61 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1501 Styrene Butadiene Rubber KRALEX® 1501 is a standard grade of styrene butadiene rubber. It is produced by a technology of cold emulsion polymerization based on soaps of rosin acids and contains 23.5% of chemically bonded .. |
|||
300% Modulus | 0.0120 - 0.0170 GPa | 1.74 - 2.47 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1712 Styrene Butadiene Rubber KRALEX® 1712 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5.. |
|||
300% Modulus | 0.0120 - 0.0180 GPa | 1.74 - 2.61 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1721 Styrene Butadiene Rubber KRALEX® 1721 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 40% .. |
|||
300% Modulus | 0.0120 - 0.0170 GPa | 1.74 - 2.47 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1723 Styrene Butadiene Rubber KRALEX® 1723 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5.. |
|||
300% Modulus | 0.0120 - 0.0180 GPa | 1.74 - 2.61 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1732 Styrene Butadiene Rubber KRALEX® 1732 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 32% .. |
|||
300% Modulus | 0.0120 - 0.0180 GPa | 1.74 - 2.61 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1739 Styrene Butadiene Rubber KRALEX® 1739 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 40% .. |
|||
300% Modulus | 0.0120 - 0.0170 GPa | 1.74 - 2.47 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1778 Styrene Butadiene Rubber KRALEX® 1778 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1490IV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1685AD Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D638 |
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D638 |
ELASTO UK Dryflex® 422501S SBS Based Material, 50D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.0120 GPa | 1.74 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |