Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0108 GPa @Temperature 145 °C, Time 2100 sec |
1.56 ksi @Temperature 293 °F, Time 0.583 hour |
cured; ASTM D412 |
LG Chemical BR 1208 Polybutadiene Polymer Description: BR1208 is high cis- 1,4 polybutadiene polymer produced by a solution polymerization process employing a stereospecific catalyst to control microstructure, molecular weight and molecular.. |
|||
300% Modulus | 0.0108 GPa @Temperature 145 °C, Time 2100 sec |
1.56 ksi @Temperature 293 °F, Time 0.583 hour |
ASTM D412 |
LG Chemical SBR 1721 High Acrylonitrile Polymer Description: SBR 1721 is an oil extended cold polymerization SBR with 37.5 parts of highly aromatic oil and styrene-butadiene copolymer of 40% bound styrene. Raw materials for this product are car.. |
|||
300% Modulus | 0.0108 GPa @Temperature 145 °C, Time 2100 sec |
1.56 ksi @Temperature 293 °F, Time 0.583 hour |
ASTM D412 |
LG Chemical SBR 1737 High Acrylonitrile Polymer Description: SBR 1737 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (PolyCyclic Aromatic) oil and styrene-butadiene copolymer of 37% bound styrene. Raw materials for this pr.. |
|||
300% Modulus | 0.0108 GPa | 1.57 ksi | |
Taiwan PU Corporation TPU-E90 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0108 GPa | 1.57 ksi | |
Taiwan PU Corporation TPU-EH90 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0108 GPa | 1.57 ksi | |
Taiwan PU Corporation TPUI-E85 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0108 GPa | 1.57 ksi | |
Taiwan PU Corporation TPUI-G85 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0108 GPa | 1.57 ksi | |
Taiwan PU Corporation TPUI-H85 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |