Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0102 GPa | 1.48 ksi | DIN 53504 |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
300% Modulus | 0.0102 GPa | 1.48 ksi | ASTM D412 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
300% Modulus | 0.0102 GPa | 1.48 ksi | ASTM D412 |
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
300% Modulus | 0.0102 GPa | 1.48 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR8020 Standard Adipate Ester Polyurethane The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGr.. |