Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | >= 0.009797 GPa | >= 1.421 ksi | ZCI-T-008 |
Zeon Chemicals Zetpol® 1010 Hydrogenated Nitrile Elastomomer Zeptol 1010 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical reistance to aggressive fluids, and an excellent balance of.. |
|||
300% Modulus | >= 0.009797 GPa | >= 1.421 ksi | ZCI-T-008 |
Zeon Chemicals Zetpol® 2010L Hydrogenated Nitrile Elastomomer Zetpol 2010L is a low-Mooney version of a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressiv.. |
|||
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.009797 GPa | 1.421 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |