Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.009225 GPa | 1.338 ksi | Perpendicular Flow; ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection .. |