Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00834 GPa | 1.21 ksi | |
Taiwan Sheen Soon Sheenthane® A8555E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |