Mechanical Properties Metric English Comments
300% Modulus 0.00590 GPa
0.856 ksi
Taiwan PU Corporation TPU-CH85 High Hydrolysis Resistance, Calender Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.00590 GPa
0.856 ksi
Taiwan PU Corporation TPUI-L70 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.00590 GPa
0.856 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
300% Modulus 0.00590 GPa
0.856 ksi
ASTM D412/D638
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane
Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solut..
300% Modulus 0.00590 GPa
0.856 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..