Mechanical Properties Metric English Comments
300% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00517 GPa
0.750 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..