Mechanical Properties Metric English Comments
300% Modulus 0.00478 GPa

@Time 7200 sec
0.693 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-85-1000 TPE
Product Description: StarXTRUDE XTR-85-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P..
300% Modulus 0.00478 GPa

@Time 7200 sec
0.693 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-90-1000 TPE
Product Description: StarXTRUDE XTR-90-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P..