Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00450 GPa | 0.653 ksi | ISO 37 |
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
300% Modulus | 0.00450 GPa | 0.653 ksi | ISO 37 |
Termopol Termoton® V2GA0065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
300% Modulus | 0.00450 GPa | 0.653 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00450 GPa | 0.653 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00450 GPa | 0.653 ksi | ISO 37 |
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
300% Modulus | 0.00450 GPa | 0.653 ksi | ASTM D638 |
ELASTO UK Mediprene™ 500750M TPE, Medical Applications, 75A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
300% Modulus | 0.00450 GPa | 0.653 ksi | ISO 37 |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |