Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00319 GPa @Time 7200 sec |
0.462 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-70-1000 TPE Product Description: StarXTRUDE XTR-70-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |