Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00279 GPa | 0.405 ksi | ASTM D3574E |
Mearthane Durethaneâ„¢ M DM-640A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
300% Modulus | 0.00279 GPa @Time 7200 sec |
0.405 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7375-1000 TPE Product Description: StarFlex P 7375-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
300% Modulus | 0.00279 GPa | 0.405 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
300% Modulus | 0.00279 GPa | 0.405 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |