Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00186 GPa | 0.270 ksi | Typical properties of film cast form toluene solution; ASTM D412 |
Kraton® D1114 P (SIS) Linear Triblock Copolymer Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: .. |
|||
300% Modulus | 0.00186 GPa @Time 7200 sec |
0.270 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 65-HR-9 TPE Product Description: StarTUFF TF 65-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |