Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00138 GPa | 0.200 ksi | Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D1111 K (SIS) Linear Block Copolymer Description: Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
300% Modulus | 0.00138 GPa | 0.200 ksi | Measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1111 K (SIS) Linear Triblock Copolymer Description: Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
300% Modulus | 0.00138 GPa | 0.200 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2730 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00138 GPa | 0.200 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2740 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00138 GPa | 0.200 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2835E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00138 GPa | 0.200 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2840E Thermoplastic Elastomer Information provided by Teknor Apex Company |