Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00108 GPa @Time 7200 sec |
0.156 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7350-1000 TPE Product Description: StarFlex P 7350-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
300% Modulus | 0.00108 GPa | 0.156 ksi | JIS K6301 |
Stellarchem 475-860N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.00108 GPa | 0.156 ksi | JIS K6301 |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.00108 GPa | 0.156 ksi | JIS K6301 |
Stellarchem AB760LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.00108 GPa | 0.156 ksi | JIS K6301 |
Stellarchem AB860EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.00108 GPa | 0.156 ksi | JIS K6301 |
Stellarchem GP-975 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.00108 GPa | 0.156 ksi | JIS K6301 |
Stellarchem LP-880 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |