Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 190 Styrene - Isoprene Block Copolymer Europrene® SOL T 190 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 16% weight and diblock content is .. |
|||
300% Modulus | 0.00100 GPa | 0.145 ksi | ISO 37 |
Termopol Termoton® V2GA1050d TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
300% Modulus | 0.00100 GPa | 0.145 ksi | Estimated value; ISO 37 |
Kraton® D0243 E (SBS) Diblock Copolymer Description: Kraton D0243 E polymer is a clear, diblock copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical form identified:Kraton D02.. |
|||
300% Modulus | 0.00100 GPa | 0.145 ksi | Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D1119 P (SIS) Linear Block Copolymer Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
300% Modulus | 0.00100 GPa @Time 7200 sec |
0.145 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7330-9000 TPE Product Description: StarFlex P 7330-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |