Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 1.72369 - 30.3369 MPa @Temperature -54.4 - 82.2 °C |
250.000 - 4400.01 psi @Temperature -66.0 - 180 °F |
Average value: 16.9 MPa Grade Count:8 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |