Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 2180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 13.0 - 15.0 MPa
1890 - 2180 psi
Acrylic, Shear; ISO 4587
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
Adhesive Bond Strength 13.0 - 15.0 MPa
1890 - 2180 psi
Aluminum, Shear; ISO 4587
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
Adhesive Bond Strength 13.0 - 15.0 MPa
1890 - 2180 psi
Aluminum, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength 13.0 - 15.0 MPa
1890 - 2180 psi
Aluminum, Shear; ISO 4587
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Adhesive Bond Strength 13.0 - 15.0 MPa
1890 - 2180 psi
Aluminum, Shear; ISO 4587
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Adhesive Bond Strength 13.0 - 15.0 MPa
1890 - 2180 psi
Aluminum, Shear; ISO 4587
Permabond 737 Cyanoacrylate, toughened
PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of..
Adhesive Bond Strength 10.0 - 15.0 MPa
1450 - 2180 psi
Grit blasted mild steel, Shear; ISO 4587
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Adhesive Bond Strength 13.0 - 15.0 MPa
1890 - 2180 psi
Aluminum, Shear; ISO 4587
Permabond 910FS Cyanoacrylate, Methyl grade
PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts..
Copyright © lookpolymers.com All Rights Reserved