Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 39.0 MPa | 5650 psi | Steel-Steel; after optimum cure |
Armstrong A-2/W Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |