Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.3297 MPa
47.82 psi
Caplinq LINQTAPE™ PIT2A
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..
Adhesive Bond Strength 0.3297 MPa
47.82 psi
Caplinq LINQTAPE™ PIT2S
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..