Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 31.0 MPa | 4500 psi | Lap shear, alum to alum, 2 hrs @ 65°C |
Tra-Con Tra-Bond 216R01 Fire Retardant Epoxy TRA-BOND 216R01 is a fast curing material with a set time of 5 to 7 minutes. Samples tested were certified to the requirements of UL94 V-O, and is RoHS compliant. TRA-BOND 216R01 develops significa.. |
|||
Adhesive Bond Strength | 31.0 MPa | 4500 psi | Lap shear, alum to alum, @ 25°C |
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s.. |
|||
Adhesive Bond Strength | 31.0 MPa | 4500 psi | |
Trelleborg Emerson & Cuming Eccobond® D 275 One-Component Fast Cure Epoxy Adhesive Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy AdhesiveSemi-rigid, high strength, fast curing, pourable, epoxy structural adhesive. Good peel strength (12 pli), Recommended for bond.. |
|||
Adhesive Bond Strength | 31.0 MPa | 4500 psi | Steel/Steel; Varies with substrates |
Loctite® 638 Maximum Strength Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Adhesive Bond Strength | 31.0 MPa @Temperature 82.2 °C |
4500 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-701 Epoxy Adhesive A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond.. |
|||
Adhesive Bond Strength | 31.0 MPa | 4500 psi | Steel-Steel; after optimum cure |
Armstrong C-7/W Epoxy Adhesive, 3:2 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Adhesive Bond Strength | 31.0 MPa | 4500 psi | Lap shear, alum to alum, 2 hrs @ 65°C |
Tra-Con Tra-Bond FS411 Fast Cure Epoxy Adhesive System TRA-BOND FS-411 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. It was designed to have low outgassing in .. |