Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, silver to silver |
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se.. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, silver to silver |
Tra-Con Tra-Bond 293-1.5T General Purpose Instrument Epoxy Adhesive-Flexible TRA-BOND 293-1.5T general purpose epoxy adhesive is designed to provide strong, semi-rigid bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. This v.. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, silver to silver |
Tra-Con Tra-Bond 293-1M General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1M general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper and brass. The 293-se.. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 342-1 Room Temperature Cure Epoxy Adhesive TRA-BOND 342-1 room temperature curing epoxy adhesive is designed for applications which require outstanding thermal shock properties. This adhesive may be used to bond semi-porous materials, such a.. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 342-3.5 Room Temperature Cure Epoxy Adhesive TRA-BOND 342-3.5 room temperature curing epoxy adhesive is designed for applications which require outstanding thermal shock properties. This adhesive may be used to bond semi-porous materials such .. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, alum to alum, 15 min @ 100°C |
Tra-Con Tra-Bond JL01 High Viscosity High Temperature Fiber Optic Adhesive TRA-BOND JL01 is a high viscosity, two-component epoxy formulation that is suggested for bonding fiber optic bundles, potting glass fibers, and terminating single or multi-channel fiber optic connec.. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, alum to alum, 30 min @ 150°C |
Tra-Con Tra-Bond JL01 High Viscosity High Temperature Fiber Optic Adhesive TRA-BOND JL01 is a high viscosity, two-component epoxy formulation that is suggested for bonding fiber optic bundles, potting glass fibers, and terminating single or multi-channel fiber optic connec.. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a .. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, silver to silver |
Tra-Con Tra-Bond 293-1T General Purpose Instrument Epoxy Adhesive-Thixotropic TRA-BOND 293-1T general purpose epoxy adhesive is designed to provide strong, semi-rigid bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. This ver.. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond Ablebond 868-7U Thixotropic Epoxy Adhesive Ablebond 868-7UNF is the unfilled version of 868-7, a nonsagging, flexible epoxy adhesive. Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Steel-Steel; after optimum cure |
Armstrong C-7/H20 Epoxy Adhesive A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Steel/Steel; Varies with substrates |
Loctite® 620 High Temperature Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Adhesive Bond Strength | 26.2 MPa | 3800 psi | Grit blasted steel |
Loctite® 480 Toughened Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |