Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 3700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 25.5 MPa
3700 psi
alum/aluminum
Resinlab® AR 4315 Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4315 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any ..
Adhesive Bond Strength 25.5 MPa
3700 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F113SC BLK High Tg Fiber Optic Epoxy Adhesive
TRA-BOND F113SC BLK is a fiber optic adhesive used for terminating ALL types of fiber optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C..
Adhesive Bond Strength 25.5 MPa
3700 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F131 High Tg Room Temperature Cure Fiber Optic Adhesive
TRA-BOND F131 is a fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus ..
Copyright © lookpolymers.com All Rights Reserved