Polymer Property : Adhesive Bond Strength = 3600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 24.8 MPa
3600 psi
Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Adhesive Bond Strength 24.8 MPa
3600 psi
Resin Technology Group 388 Metals, Small Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 388 Metals, Small Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Adhesive Bond Strength 24.8 MPa
3600 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Bond 216R01 Fire Retardant Epoxy
TRA-BOND 216R01 is a fast curing material with a set time of 5 to 7 minutes. Samples tested were certified to the requirements of UL94 V-O, and is RoHS compliant. TRA-BOND 216R01 develops significa..
Adhesive Bond Strength 24.8 MPa
3600 psi
Grit blasted steel
Loctite® 493 General Purpose Methyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 24.8 MPa
3600 psi
Grit blasted steel
Loctite® 496 General Purpose Methyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 24.8 MPa
3600 psi
Grit blasted steel
Loctite® PRISM® 4210 Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 24.8 MPa
3600 psi
Grit blasted steel
Loctite® Super Bonder® 430 Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength 24.8 MPa

@Temperature 25.0 °C
3600 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-7 Epoxy Adhesive
Clear, flexible, 5-minute cure structural bonding plastic adhesive. Develops high performance, high impact durable bonds for operating temperatures from -65° to +250°. Supplied in 1:1 ratio dispe..
Adhesive Bond Strength 24.8 MPa

@Temperature 25.0 °C
3600 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong C-7/W Epoxy Adhesive, 3:2 Mix Ratio
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
Adhesive Bond Strength 24.8 MPa
3600 psi
Grit blasted steel
Loctite® 415 General Purpose Methyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..