Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.210 MPa @Temperature 23.9 °C |
30.5 psi @Temperature 75.0 °F |
Maple to itself at 50% R.H. Test at 0.1 inches/min. separation rate. |
3M Scotch-Grip™/Fastbond™ 5497 Industrial Adhesive
(discontinued **) An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.One part, 100% solids moisture curing liquid urethane adhesive which ca.. |