Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 16.9 MPa | 2450 psi | lap shear; ASTM D1002 |
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive, Grey / Beads Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 16.9 MPa | 2450 psi | ASTM D4541 |
Chesterton ARC MXC Castable Extreme Wear Compound Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro.. |
|||
Adhesive Bond Strength | 16.9 MPa @Temperature -54.4 °C |
2450 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-7 Epoxy Adhesive Clear, flexible, 5-minute cure structural bonding plastic adhesive. Develops high performance, high impact durable bonds for operating temperatures from -65° to +250°. Supplied in 1:1 ratio dispe.. |
|||
Adhesive Bond Strength | 16.9 MPa @Temperature -54.4 °C |
2450 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-1/H20 Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Adhesive Bond Strength | 16.9 MPa @Temperature -54.4 °C |
2450 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-4/W Epoxy Adhesive A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved .. |