Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Adhesive Bond Strength | 15.9 - 27.6 MPa | 2300 - 4000 psi | Average value: 20.2 MPa Grade Count:4 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t.. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi.. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c.. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond 216E02 Encapsulant for "Fill" Applications TRA-BOND 216E02 is a two-part epoxy adhesive developed specifically for underfill and encapsulating applications where the combination of excellent mechanical, thermal and electrical properties are .. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Wear Guard (High Temp) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-347 Low Expansion Epoxy Adhesive EB-347 is a highly filled, low coefficient expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensiona.. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature 82.2 °C |
2300 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-1/V Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature -54.4 °C |
2300 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-2/E Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature 82.2 °C |
2300 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-271 Epoxy Adhesive A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled .. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature -54.4 °C |
2300 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-271 Epoxy Adhesive A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled .. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature -54.4 °C |
2300 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-40 Epoxy Adhesive Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re.. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Adhesive Bond Strength | 15.9 MPa | 2300 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |