Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 14.1 MPa | 2050 psi | Polyester-Polyester; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Adhesive Bond Strength | 14.1 MPa @Temperature -54.4 °C |
2050 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-2/A Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Adhesive Bond Strength | 14.1 MPa @Temperature 25.0 °C |
2050 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-5/A Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 14.1 MPa @Temperature 25.0 °C |
2050 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-7/H20 Epoxy Adhesive A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Adhesive Bond Strength | 14.1 MPa @Temperature -54.4 °C |
2050 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong X-81-A/F Epoxy Adhesive Information provided by Ellsworth Adhesives. |