Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 12.1 MPa | 1750 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t.. |
|||
Adhesive Bond Strength | 12.1 MPa | 1750 psi | Lap shear, alum to alum |
Tra-Con Tra-Duct 2979 Microelectronic Conductive Epoxy Adhesive TRA-DUCT 2979 is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid t.. |
|||
Adhesive Bond Strength | 12.1 MPa | 1750 psi | Lap shear, alum to alum |
Tra-Con Tra-Duct 2979LV Microelectronic Conductive Epoxy Adhesive TRA-DUCT 2979LV is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid.. |
|||
Adhesive Bond Strength | 12.1 MPa @Temperature 25.0 °C |
1750 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-2/H20 Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Adhesive Bond Strength | 12.1 MPa @Temperature -54.4 °C |
1750 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-5/A Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 12.1 MPa @Temperature -54.4 °C |
1750 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong X-81/A Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 12.1 MPa | 1750 psi | uncured |
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o.. |
|||
Adhesive Bond Strength | >= 12.1 MPa | >= 1750 psi | Dry concrete; ASTM D4541 |
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer Description: An advanced composite formulated to protect concrete surfaces from mild chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat. Non-shrinking. 1.. |